International Scholarly Research Notices Hindawi
The time of milling varies from 1 h to 11 h depending upon the rate of formation of Mg ferrite phase The 9 h ball milled powder was postannealed at 873 973 and K successively each for 1 h duration in air in a programmable furnace with 5 K/min and 20 K/min heating and cooling rates respectively